The present invention relates to a method for the recrystallizing annealing of a non-grain-oriented electrical steel strip (2) in a continuous annealing and coating line (1) Heating rate of at least 80 K / s and then, if necessary, a second continuous furnace (8) is heated to a temperature of at least 820 ° C with a heating rate of a maximum of 20 K / s, with the electrical steel strip (2) in front of the induction furnace (5) is first heated to a temperature of at least 300 ° C. with a heating rate of a maximum of 60 K / s via a first continuous furnace (3).
机译:本发明涉及一种在连续退火和涂布管线(1)加热速率下重结晶的非谷物取向的电钢带(2)的退火的方法,其中至少80k / s,然后,如有必要,a 第二连续炉(8)被加热至至少820℃的温度,加热速率最大为20k / s,电钢带(2)在感应炉(5)的前面是首先加热 温度至少为300℃。通过第一连续炉(3),最大为60k / s的加热速率。

著录项

  • 公开/公告号DE102021201616A1

    专利类型

  • 公开/公告日2021-12-02

    原文格式PDF

  • 申请/专利权人 SMS GROUP GMBH;

    申请/专利号DE202110201616

  • 申请日2021-02-19

  • 分类号C21D8/12;C21D9;C21D1/26;C21D1;

  • 国家 DE