The invention relates to a method for patinating zinc surfaces of a structural element, comprising the steps of: - providing a structural element with a zinc surface in a housing; - providing an atmosphere around the zinc surface, wherein said atmosphere comprises carbon based gas and humidity; and - heating the zinc surface for at least one hour, to provide a patinated zinc surface, wherein the heating of the zinc surface occurs by heating the atmosphere to a temperature of at least 50 °C, the humidity is at least 70%, and the carbon based gas concentration is at least 5% by volume. The invention also relates to a patinated evaporative condenser in a closed circuit cooling tower, wherein the patinated evaporative condenser in a closed circuit cooling tower is by the method according to the invention. The invention also relates to a system for patinating zinc surfaces according to the invention.
机译:本发明涉及一种用于图案化结构元件锌表面的方法,包括以下步骤: - 在壳体中提供具有锌表面的结构元件; - 提供锌表面周围的气氛,其中所述大气层包括基于碳的气体和湿度; 和 - 加热锌表面至少1小时,提供镀锌锌表面,其中通过将气氛加热至至少50℃的温度,湿度至少为70%,发生锌表面的加热,并且 碳基气体浓度至少为5重量%。 本发明还涉及封闭式电路冷却塔中的镀透明的蒸发冷凝器,其中闭合电路冷却塔中的镀饰蒸发冷凝器是根据本发明的方法。 本发明还涉及一种用于图案化根据本发明的锌表面的系统。

著录项

  • 公开/公告号EP3899080A1

    专利类型

  • 公开/公告日2021-10-27

    原文格式PDF

  • 申请/专利权人 AQUACARE EUROPE B.V.;

    申请/专利号EP20190835544

  • 发明设计人 BAAS KOOS JAN;

    申请日2019-12-20

  • 分类号C23C2/26;C23C8/02;C23C8/16;C23C8/20;C23C8/28;C23C8/34;

  • 国家 EP

  • 入库时间 2022-08-24 21:55:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号