METHOD FOR PROCESSING TITANIUM AND ITS ALLOYS IN ORDER TO INCREASE ITS CORROSION RESISTANCE AND ELECTROLYTE FOR MICRO-ARC OXIDATION OF TITANIUM AND ITS ALLOYS IN ORDER TO INCREASE CORROSION RESISTANCE

机译:加工钛及其合金的方法,以提高钛及其合金微弧氧化的耐腐蚀性和电解质,以提高耐腐蚀性

摘要

FIELD: electroplating.;SUBSTANCE: invention relates to the field of electroplating and can be used in various fields of technology, as well as in the chemical industry and electrochemical industries. The method includes microarc oxidation in a KOH solution at a forming voltage of 500-550 V, anodic-cathodic mode with a frequency of 50 Hz, with equal anodic and cathodic currents and a current density of 45 A/dm2, while microarc oxidation is carried out in an electrolyte containing 3 g/l of KOH and 1-5 g/l of heptahydrate nickel sulfate NiSO4 ⋅ 7H2O, with a duration of microarc oxidation of at least 10 minutes. The electrolyte contains 3 g/l of KOH and 1-5 g/l of heptahydrate nickel sulfate NiSO4 ⋅ 7H2O. The advantages of the proposed coating are low cost, because does not require bulk alloying and surface alloying of titanium, relative ease of production and low energy consumption due to the short deposition time.;EFFECT: increasing the corrosion resistance of titanium and its alloys.;2 cl, 3 tbl
机译:田地:电镀。物质:发明涉及电镀领域,可用于各种技术领域,以及化学工业和电化学行业。该方法包括以500-550V,阳极 - 阴极模式的成形电压,频率为50Hz的阳极和阴极电流,电流密度为45a / dm2,而Microarc氧化是在含有3g / L KOH的电解质和1-5g / L的七水合物硫酸镍NISO 4×7H2O的电解质中进行,持续时间氧化至少10分钟。电解质含有3g / L的KOH和1-5g / L的七水合物硫酸镍NISO4⋅7H2O。所提出的涂层的优点是成本低,因为由于短的沉积时间,不需要批量合金化和钛的表面合金化,相对容易的生产和低能量消耗。;效果:提高钛及其合金的耐腐蚀性。 ; 2 cl,3 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号