FIELD: road-building mixtures. ;SUBSTANCE: invention relates to the field of road-building mixtures, in particular to the production of modern material for road surfaces with improved physical and mechanical properties. The mixture includes the following components: a composite binder of one bitumen of the first row - CB (Construction Bitumen) 90/130, CB 60/90, CB 40/60 together with one of the bitumen of the second row - CB 200/300, CB 130/200 with a predominance of the first row bitumen in the binder; composite reinforcing fibromaterial of polyacrylonitrile (PAN) and basalt fibers with a predominance of PAN fibers in the fibromaterial; mineral powder, sand. The components are contained in the following ratio: reclaimed crushed asphalt concrete and mineral powder formed from particles with a size of not more than 1.25 mm of reclaimed crushed asphalt concrete, and constituting 10-20% of the amount of the latter in the total amount - 24-25%. Composite binder, in which bitumen of the first and second rows are presented as follows: bitumen of the first row - 85-95%, that of the second row - 5-15% - in a total amount of 4-8%, oleic acid 0.2-0.6%, composite reinforcing fibromaterial in the amount of 0.15-0.7%, in which PAN is 60-95%, basalt fiber - 5-40%. Sand is the rest. ;EFFECT: improvement of the physical and mechanical strength characteristics of asphalt concrete, in particular those of water resistance and shear resistance. ;1 cl, 2 tbl, 1 ex
机译:领域:道路建设混合物。 ;物质:发明涉及道路建筑混合物领域,特别是具有改进的物理和机械性能的道路表面的现代材料的生产。该混合物包括以下组分:第一排 - Cb(施工沥青)90/130,CB 60/90,CB 40/60的一个复合粘合剂以及第二行的沥青的一个沥青 - CB 200 / 300,CB 130/200具有粘合剂中的第一行沥青的优势;聚丙烯腈(锅)和玄武岩纤维的复合增强纤维材料,纤维纤维纤维材料的优势;矿物粉,沙子。该组分以下列比率含有:回收碎屑沥青混凝土和矿物粉末,由尺寸不超过1.25mm的再生碎沥青混凝土形成,并在总量中构成后者的10-20% - 24-25%。复合粘合剂,其中第一行和第二行的沥青如下:第一行的沥青 - 85-95%,第二行的沥青 - 5-15% - 总量为4-8%,油酸0.2-0.6%,复合增强纤维材料的量为0.15-0.7%,其中锅为60-95%,玄武岩纤维 - 5-40%。沙子是其余的。 ;效果:改善沥青混凝土的物理和机械强度特性,特别是耐水性和抗剪切抗性。 ; 1 cl,2 tbl,1前

著录项

  • 公开/公告号RU2751628C1

    专利类型

  • 公开/公告日2021-07-15

    原文格式PDF

  • 申请/专利权人

    申请/专利号RU2020109111

  • 发明设计人 ANDRONOV SERGEI IUREVICH (RU);

    申请日2020-03-02

  • 分类号C04B26/26;C08L95;C04B111/20;C04B111/27;

  • 国家 RU

  • 入库时间 2022-08-24 20:07:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号