A multi-scale and multi-phase dispersion strengthened iron-based alloy, and preparation and characterization methods thereof are provided. The alloy contains a matrix and a strengthening phase. The strengthening phase includes at least two types of the strengthening phase particles with different sizes. A volume of the two types of the strengthening phase particles with different sizes having a particle size less than or equal to 50 nm accounts for 85-95% of a total volume of all the strengthening phase particles. The matrix is a Fe—Cr—W—Ti alloy. The strengthening phases include crystalline Y2O3 phase, Y—Ti—O phase, Y—Cr—O phase, and Y—W—O phase. The characterization method comprises electrolytically separating the strengthening phases in the alloy, and then characterizing by using an electron microscope. The tensile strength of the prepared alloy is more than 1600 MPa at room temperature, and is more than 600 MPa at 700° C.
机译:多尺度和多相色散强化铁基合金,并提供了其制备和表征方法。合金含有基质和强化相。强化相包括具有不同尺寸的至少两种强化相颗粒。具有粒径小于或等于50nm的不同尺寸的两种强化相颗粒的体积占所有加强相颗粒的总体积的85-95%。基质是Fe-Cr-W-Ti合金。强化阶段包括结晶Y 2℃ O 3 相,Y-Ti-O相,Y-CR-O相和Y-W-O相。表征方法包括在合金中电解分离强化阶段,然后通过使用电子显微镜表征。制备合金的拉伸强度在室温下大于1600MPa,在700℃下大于600MPa。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号