FIELD: working of metals.;SUBSTANCE: invention relates to methods of production of sintered products from lead bronze powders and can be used in manufacture of products for general mechanical engineering purposes. The method for production of sintered products from lead bronze powders includes pressing the bronze powder and sintering the pressed material producing a sintered product. Nano-sized spherical lead bronze powder produced by electroerosive dispersion of lead bronze waste in distilled water is subjected to pressing at a pulse repetition rate of 95 to 105 Hz, voltage on the electrodes of 190 to 200 V and capacitance of 65.5 mcF, the powder is pressed by monoaxial pressing at a pressure of 1500 MPa with exposure of 2 minutes, and the pressed material is sintered at a temperature of 827°C in an argon medium for 12 hours. ;EFFECT: reduced porosity and increased hardness of sintered products are ensured.;1 cl, 6 dwg, 3 ex
机译:现场:金属的工作。;物质:发明涉及来自铅青铜粉末的烧结产品的方法,可用于制造产品以进行一般机械工程目的。来自铅青铜粉末的烧结产品的制备方法包括压制青铜粉末并烧结制造烧结产物的压制材料。通过在蒸馏水中的铅青铜废物的铅青铜废物的电子分散体产生的纳米球铅青铜粉末在脉冲重复率为95至105Hz,电极上的电压为190至200 V,电容为65.5mcf,粉末通过在1500MPa的压力下通过曝光2分钟的压力压制,并将压制材料在827℃的温度下在氩气培养基中烧结12小时。 ;效果:确保了降低的孔隙率和增加的烧结产品硬度。; 1 cl,6 dwg,3前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号