FIELD: environmental protection; oil and gas production industry.;SUBSTANCE: method involves preparation of a recycling product by mixing drilling mud, sand, cement and sorbent at the following ratio of components, wt %: drilling mud 50, cement 2–5, sorbent 2–5, sand—the rest. Prior to pumping, the recycling product is transferred into a movable state with introduction of liquid into it to moisture content of 20–60 %, wherein the working temperature of the obtained recycling product must be not less than 30 °C, and ambient temperature during pumping of recycling product is not lower than 5 °C. Obtained recycling product is pumped into the liquidated underground storage through the first production well bore, after which fluid is displaced from underground storage to second production well, wherein displaced liquid is used during subsequent transfer of recycling product into mobile state, process of underground storage filling is performed before displacement of injected recycling product is started from the second production well. At that, control of underground storage filling quality is carried out, for this purpose on day surface at least two control wells are drilled, after that, pumping process is resumed until complete pumping of pumped recovery product from all drilled wells. Finally, each said well is sealed by grouting of the shafts and bottomhole zones.;EFFECT: similar solution prevents negative impact on environment.;8 cl, 1 dwg, 2 tbl
机译:领域:环境保护;石油和天然气生产行业。物质:方法:方法涉及通过将钻井泥浆,砂,水泥和吸附剂的组分的比例混合,Wt%:钻井泥浆50,水泥2-5,吸附剂2-5,沙子 - 其余的。在泵送之前,将再循环产物转移到可移动状态中,以将液体引入到其中的水分含量为20-60%,其中所获得的再循环产物的工作温度必须不小于30℃和环境温度泵送回收产品不低于5°C。将获得的再循环产物通过第一生产井孔泵入清除地下储存,之后将流体从地下储存到第二生产井中,其中在随后将回收产品转移到移动状态下,地下储存填充过程中使用移位液体在注入的再循环产品的位移之前进行从第二种生产井开始进行。此时,为此目的,对地下储存填充质量进行控制,在日表面上钻出至少两个控制孔,之后,恢复泵送过程直到从所有钻井的泵浦回收产品完全泵送。最后,每个所述井通过竖井和底孔区域灌浆密封。;效果:类似的解决方案可以防止对环境产生负面影响。; 8 Cl,1 dwg,2 tbl

著录项

  • 公开/公告号RU2746918C2

    专利类型

  • 公开/公告日2021-04-22

    原文格式PDF

  • 申请/专利权人

    申请/专利号RU20180140798

  • 发明设计人 PERMINOV VLADIMIR ALEKSEEVICH (RU);

    申请日2018-11-19

  • 分类号E21F17/16;

  • 国家 RU

  • 入库时间 2022-08-24 18:22:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号