A procedure to separate the sulfur and the iron contained in mixtures of sulfide mineral and aqueous solutions of sulfuric acid (Machine-translation by Google Translate, not legally binding)

机译:分离硫化物矿物和硫酸水溶液中所含硫和铁的程序(由Google Translate进行机器翻译,不具有法律约束力)

摘要

A process of separating sulfur and iron contained in mixtures of sulfide ore and aqueous solutions of sulfuric acid, comprising; 1) heat treating a sulfide mixture at temperatures below the melting temperature of the mixture in the presence of metallic iron to render the iron content substantially completely reactive with sulfuric acid to produce iron sulfate and gaseous hydrogen sulfide; 2) reacting the treated sulphide ore mixture with the acidic content of a sulfuric acid solution to produce a suspension containing gaseous hydrogen sulfide, solids containing the insoluble components of the feed and those impurities from the solution whose salts sulfur are insoluble in the solution in the presence of hydrogen sulfide gas, a neutral solution containing iron sulfate, at concentrations lower than saturation at 65º C, and those impurities from the feed materials that are soluble in the solution; 3) recover the gaseous hydrogen sulfide produced; 4) separating the insoluble solids from the neutral solution; 5) separating water from the neutral filtrate at temperatures below 64.8º C to produce solutions that are substantially saturated with iron sulfate at about 64.8º C; 6) heating the saturated solution with live steam from temperatures of about 64.8º C to temperatures substantially above 64.8º C to precipitate iron sulfate crystals monohydrate; and 7) separating the iron sulfate crystals monohydrate at a temperature above about 64.8º C. (Machine-translation by Google Translate, not legally binding)
机译:一种分离硫化矿石和硫酸水溶液混合物中所含硫和铁的方法,包括: 1)在金属铁的存在下,在低于混合物的熔融温度的温度下热处理硫化物混合物,以使铁含量基本上完全与硫酸反应,产生硫酸铁和气态硫化氢; 2)使处理过的硫化矿矿石混合物与硫酸溶液的酸性成分反应,制得含有气态硫化氢的悬浮液,含有进料不溶成分的固体以及溶液中盐硫不溶的那些杂质。存在硫化氢气体,浓度低于65ºC的饱和度的含硫酸铁的中性溶液,以及来自进料的可溶于该溶液的杂质; 3)回收产生的气态硫化氢; 4)从中性溶液中分离出不溶性固体; 5)在低于64.8℃的温度下从中性滤液中分离出水,以产生在约64.8℃下基本上被硫酸铁饱和的溶液; 6)用新鲜蒸汽将饱和溶液从约64.8ºC加热到实质上高于64.8ºC,以沉淀出硫酸铁晶体一水合物;和7)在高于约64.8ºC的温度下分离一水合硫酸铁晶体。(由Google Translate进行的机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES286248A1

    专利类型

  • 公开/公告日1963-08-01

    原文格式PDF

  • 申请/专利权人 CHEMETALS CORPORATION;

    申请/专利号ES19630286248

  • 发明设计人

    申请日1963-03-20

  • 分类号1B01A;1C22B;

  • 国家 ES

  • 入库时间 2022-08-23 17:23:52