首页> 外国专利> A procedure for the manufacture of steels of improved suitability for the mechanization with lifting of chips. (Machine-translation by Google Translate, not legally binding)

A procedure for the manufacture of steels of improved suitability for the mechanization with lifting of chips. (Machine-translation by Google Translate, not legally binding)

机译:一种提高了切屑提升机械化适应性的钢的制造过程。 (通过Google翻译进行机器翻译,没有法律约束力)

摘要

A method for the manufacture of steel of improved aptitude for machining with shavings, characterized in that from a previous material of the desired steel, containing at least one alloy element, soluble in the liquid steel and improving the For machining with chip removal, an ingot is produced according to the electrical remelting procedure using slag, which consists of 10 to 40% Al2O3, in addition to alkaline earth metal oxides, preferably CaO in amounts between 0 and 40% and/or of CaF2 in quantities between 10 and 70%, as well as 10 to 50% of SiO2, with the proviso that, as there are oxides of alkaline earth metals, the minimum content in itself O2, amounts to 1.1 times the content of alkaline earth metal oxides and that the sum of the unavoidable impurities of the slag does not exceed the proportion of 10%. (Machine-translation by Google Translate, not legally binding)
机译:一种用于制造具有刨花加工性能的钢的方法,其特征在于,由所需钢的先前材料制成,该材料包含至少一种可溶于液态钢的合金元素,并改善了切削性能。该产品是根据电重熔程序使用炉渣生产的,除碱土金属氧化物外,炉渣还包含10%至40%的Al2O3,CaO的含量优选为0%至40%,和/或CaF2的含量为10%至70%,以及10%到50%的SiO2,但前提是,由于存在碱土金属的氧化物,因此O2本身的最低含量为碱土金属氧化物的1.1倍,并且不可避免的杂质之和渣的比例不超过10%。 (通过Google翻译进行机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES334067A1

    专利类型

  • 公开/公告日1967-10-16

    原文格式PDF

  • 申请/专利权人 GEBR. BOHLER & CO. A.G.;

    申请/专利号ES19660334067

  • 发明设计人

    申请日1966-12-02

  • 分类号C22B9/18;C22C38/60;

  • 国家 ES