Ethylene copolymers contg. 60% wt. ethylene, 1-15% wt. (meth)acrylic acid, and 0.5-20%wt. of an ester of (meth)arcylic acid with a primary 1-12C alcohol and opt. up to 1.0% wt. t-butyl (meth)acrylate are prepd. by (a) polymerising a mixt. of 100pts. wt. ethylene, 0.1-5 pts. wt. of an ester of (meth)acrylic acid with a primary 1-12C alcohol, and 0.3-4.5 pts. wt. t-butyl (meth)acrylate, at 200-270 degrees C and 1000-8000 atm. and a residence time of 40-120 secs. using a catalytic amount of a free radical initiator, and (b) exposing the reaction mixt. for 40-90 secs. to a temp. of 280-320 degrees C. Polymsn. is pref. effected in the presence of 0.2-5% vol. based on ethylene of a polymsn. regulator. Used as adhesives for prodn. of laminates.
机译:乙烯共聚物续> 60%重量乙烯,1-15%wt。 (甲基)丙烯酸,和0.5-20重量%。 (甲基)水杨酸与1-12C伯醇的酯的合成最高1.0%wt。制备(甲基)丙烯酸叔丁酯。通过(a)聚合混合物。 100pts。重量乙烯,0.1-5点。重量(甲基)丙烯酸与1-12C伯醇的酯,量为0.3-4.5磅。重量(甲基)丙烯酸叔丁酯,在200-270摄氏度和1000-8000大气压下。停留时间为40-120秒。使用催化量的自由基引发剂,和(b)暴露反应混合物。持续40-90秒。暂时280-320℃。是首选。在0.2-5%体积的存在下进行。基于polymsn的乙烯。调节器。用作产品的粘合剂。层压板。

著录项

  • 公开/公告号DE2119047A1

    专利类型

  • 公开/公告日1972-11-09

    原文格式PDF

  • 申请/专利权人

    申请/专利号DE19712119047

  • 发明设计人

    申请日1971-04-20

  • 分类号C08F210/02;

  • 国家 DE

  • 入库时间 2022-08-23 08:19:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号