White devitrified glass fabrication by elaborating a glass of the CaO-MgO Al2O3-SiO2 system casting the molten glass opacified by phase separation and forming a sheet of glass which is devitrified by heating stearate of 5-10 degrees C/min. up to 1050-1080 degrees C, holding at this temp. for 1 hr (max) then cooling to the vitrifying temp. Cheaper raw products e.g. sand limestone/chalk, dolomite and soda can be used.
机译:通过制作CaO-MgO Al2O3-SiO2系统的玻璃,浇铸通过相分离而变得不透明的熔融玻璃,并形成一块玻璃片,进行白色失透玻璃的制造,该玻璃片通过加热5-10℃/ min的硬脂酸盐来失透。保持在1050-1080摄氏度。保持1小时(最大),然后冷却至玻璃化温度。便宜的原始产品,例如可以使用砂石灰石/粉笔,白云石和苏打水。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号