process for the reduction of the content of iron and sulfur in the slag of blast furnace and slag raf finata obtained useful, in particular, for the production of glass ceramics and the like

机译:所获得的降低高炉炉渣和矿渣浮渣中铁和硫含量的方法,特别适用于玻璃陶瓷等的生产

摘要

1428154 Treating slags CALUMITE CO 11 Sept 1973 [12 Sept 1972] 42637/73 Headings C1K C1A and C1M Slag, -12 U.S. mesh size, is heated to at least 400‹ F. but below fusion in the presence of air and whilst being agitated to reduce its sulphur content, preferably to below 0À3%. Its iron content can also be reduced by simultaneously or successively adding a chlorine liberating compound. The product can be mixed with glass forming materials or sand with either recycled glass or gypsum to give a flint glass. The SO 2 formed in producing the slag can be introduced into the glass melt during glass making.
机译:1428154处理炉渣1973年9月11日[1972年9月12日] 42637/73标题C1K C1A和C1M炉渣,美国筛分尺寸为-12,被加热到至少400?F,但在有空气和搅拌的情况下低于熔融温度。以降低其硫含量,最好降低到0‑3%以下。同时或相继加入释放氯的化合物也可以降低其铁含量。该产品可以与玻璃成型材料混合,也可以与沙子与再生玻璃或石膏混合,制成火石玻璃。在制造炉渣时形成的SO 2可以在玻璃制造过程中引入到玻璃熔体中。

著录项

  • 公开/公告号IT996159B

    专利类型

  • 公开/公告日1975-12-10

    原文格式PDF

  • 申请/专利权人 HORKINS J;

    申请/专利号IT19730052466

  • 发明设计人

    申请日1973-09-11

  • 分类号C03C;

  • 国家 IT

  • 入库时间 2022-08-23 02:39:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号