Procedure for precipitating zinc oxyhydroxide suitable for electrolysis from zinc chloride solutions, in particular, those obtained by elution in the process of ionic exchange of lyes from wet treatment of different minerals and pyritic products, such as the ashes of roasting of sulphated or chlorinated pyritic minerals, and of the solutions obtained in the retention of volatile chlorides in the treatments of chloridation volatilization, characterized in that the acid solution of zinc chloride is added, at a temperature of 50- 60º, an alkali to neutralize the free acidity, then adding ammonia, gaseous or in aqueous solution, to precipitate the zinc in the form of zinc hydroxide, after which the suspension is heated to 95-100ºC to optimize the precipitation yields, separating, finally, the precipitate of zinc oxyhydroxide, suitable for the production of zinc electrolyte ico (Machine-translation by Google Translate, not legally binding)
机译:从氯化锌溶液中沉淀适合于电解的氢氧化正锌的沉淀程序,特别是通过对不同矿物和黄铁矿产品进行湿处理而在碱液的离子交换过程中洗脱得到的溶液,例如,焙烧硫酸或氯化黄铁矿的灰烬,以及在氯化挥发处理中保留挥发性氯化物得到的溶液中,其特征在于,在50-60ºC的温度下加入碱金属的氯化锌以中和游离酸度,然后加入氨水,气态或水溶液形式,以氢氧化锌形式沉淀锌,然后将悬浮液加热至95-100ºC以优化沉淀产率,最后分离出氢氧化锌沉淀,适合用于生产锌电解质ico(Google翻译的机器翻译,不具有法律约束力)

著录项

  • 公开/公告号ES432943A1

    专利类型

  • 公开/公告日1976-10-01

    原文格式PDF

  • 申请/专利权人 EMPRESA AUXILIAR DE LA INDUSTRIA S. A.;

    申请/专利号ES19740432943

  • 发明设计人

    申请日1974-12-14

  • 分类号C22B;C25C;

  • 国家 ES

  • 入库时间 2022-08-23 02:27:44

相似文献

  • 专利
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号