An improved method for preparing a catalytic composition that includes a calcined alumina aggregate in admixture with oxides that impart stability at high temperatures, which method comprises: forming an intimate mixture comprising an alumina-producing aluminum compound and, at least, two additional metal compounds, which on calcination provide the corresponding metal oxides, said metal compounds being composed of metals selected from the group consisting of a) chromium or tungsten or mixtures thereof and, at least, a metal of group ivb; b) a metal of the rare earths and, at least, a metal of group ivb; c) a metal of the rare earths and as or tungsten or mixtures thereof; d) a metal of the rare earths, chromium or tungsten or mixtures thereof and, in addition, at least one metal of group ivb, and e) a metal of the rare earths, chromium or tungsten or mixtures thereof and, in addition,, calcium, strontium, barium, silicon, tin or mixtures thereof; calcining said intimate mixture at a temperature of at least 850º c, except for the oxidic component e) which is subjected to 500º c, to form an oxidic and catalytically active aggregate thereof, characterized by a surface area of, at least, 20 m2/g, after calcination for 2 hours at 1,200º c; and incorporating a catalytically effective amount of a metal from the platinum group into said calcined mixture. (Machine-translation by Google Translate, not legally binding)
机译:一种改进的制备催化剂组合物的方法,该方法包括将煅烧的氧化铝聚集体与可在高温下提供稳定性的氧化物混合,该方法包括:形成紧密混合物,该混合物包含产生氧化铝的铝化合物和至少两种其他金属化合物,在煅烧时提供相应的金属氧化物,所述金属化合物由选自以下的金属组成:a)铬或钨或它们的混合物,以及至少ivb族的金属; b)稀土金属,至少是ivb族金属; c)稀土金属和/或钨或它们的混合物; d)稀土金属,铬或钨的金属或其混合物,以及至少一种ivb组的金属,以及e)稀土金属,铬或钨的金属或其混合物,并且,钙,锶,钡,硅,锡或它们的混合物;在至少850°C的温度下煅烧所述紧密混合物,但要经受500°C的氧化组分e)除外,以形成其氧化和催化活性的聚集体,其特征是表面积至少为20 m2 / g,在1200℃下煅烧2小时后;将催化有效量的铂族金属引入到所述煅烧混合物中。 (通过Google翻译进行机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES432719A1

    专利类型

  • 公开/公告日1977-02-16

    原文格式PDF

  • 申请/专利权人 ENGELHARD MINERALS & CHEMICALS CORPORATION;

    申请/专利号ES19740432719

  • 发明设计人

    申请日1974-12-09

  • 分类号B01J;

  • 国家 ES

  • 入库时间 2022-08-23 00:30:55

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号