首页> 外国专利> Zeolite mouldings contg. basic aluminium chloride binders - produced with flowable zeolite powders contg. water and with amorphous binder

Zeolite mouldings contg. basic aluminium chloride binders - produced with flowable zeolite powders contg. water and with amorphous binder

机译:沸石成型品续。碱性氯化铝粘合剂-用可流动的沸石粉续制。水和无定形粘合剂

摘要

Zeolite mouldings contg. basic Al chloride binders are produced by mixing zeolite powder with binder, kneading moulding mixt. opt. with addn. of water, and calcining at =500 degrees C. Zeolite powder used is capable of flowing and contains 40-70 wt.% water. Basic Al chloride is prepd. by treating aq. solns. contg. Al and Cl ions with solns. of amines having mol.wt. 250-500 in a water-immiscible organic solvent. The aq. and organic phase are then sepd. from one another. The basic Al chloride is recovered from sepd. aq phase by a standard method, provided that the aq. soln. contains max. 25g/l Al and the organic phase contains max. 0.35 mol/l amine. Amorphous basic Al chloride used in an excellent binder for zeolite moulding prodn. Mouldings obtd. have good absorption and catalytic properties.
机译:沸石成型品续。碱性氯化铝粘合剂是通过将沸石粉末与粘合剂混合,捏合成型混合物而制得的。选择。与addn。的水,并在= 500摄氏度下煅烧。所用的沸石粉末能够流动,并且包含40-70 wt。%的水。制备碱性氯化铝。通过处理水solns。续铝和氯离子与锡。具有摩尔重量的胺。在与水不混溶的有机溶剂中250-500。水溶液然后分离有机相。彼此之间。从sepd中回收碱性氯化铝。 aq相采用标准方法,条件是aq。 soln。最多25g / l的铝和有机相含有最大0.35 mol / l胺。非晶态碱性氯化铝,用于沸石成型产品的优异粘合剂中。模制品。具有良好的吸收和催化性能。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号