Recovery of a solid vanadate cpd. from its aq. soln. is effected by spray drying into a zone at 300-750 (400-550) degrees C and rapid chilling of the fine vanadate particles formed to a temp. 250 (150) degrees C. The V recovery is high and the process avoids the formation of contaminated liq. effluents, as occurs when ammonium vanadate is obtd. by crystallisation. In an example, 1 l aq. (NH4)6V10O28 soln. (7.91 wt.% V2O5) were spray dried, using 333 ml/min. soln. at 47 degrees C and 1.6 ft3/min. combustion gas at an inlet temp. of 480 degrees C and an outlet temp. of 128 degrees C. The (NH4)6V10O28 recovery was 91%.
展开▼
机译:回收固体钒酸盐cpd。从它的水soln。通过在300-750(400-550)℃下将其喷雾干燥到一个区域中,并将形成的细钒酸盐微粒快速冷却至一定温度来进行。 250(150)摄氏度。V回收率高,并且该过程避免了污染液体的形成。废水,如钒酸铵过剩时发生的情况。通过结晶。在一个示例中,为1 l aq。 (NH4)6V10O28溶液。用333毫升/分钟将(7.91重量%的V 2 O 5)喷雾干燥。 soln。在47摄氏度和1.6立方英尺/分钟的速度下。进气温度下的燃烧气体。 480摄氏度和出口温度。熔点为128℃。(NH 4)6 V 10 O 28的回收率为91%。
展开▼