ABSTRACTEpoxy novolac resins having a narrow molecularweight distribution are prepared by dissolving an epoxynovolac resin prepared by conventional means in a suitablesolvent such as xylene, cooling below 50°C until separationinto 2 phases occurs, separating the two phases and removingthe solvent therefrom thereby producing a resin of relativelylow molecular weight and a resin of relatively high molecularweight wherein each resin has a narrow molecular weightdistribution.
机译:抽象分子窄的环氧线型酚醛树脂通过溶解环氧树脂制备重量分布通过常规方法以合适的方式制备线型酚醛树脂溶剂(例如二甲苯),冷却至50°C以下直至分离分为两个阶段,将两个阶段分离并移除由此产生溶剂,从而产生相对低分子量和较高分子量的树脂每种树脂的分子量较窄的重量分配。

著录项

  • 公开/公告号CA1038994A

    专利类型

  • 公开/公告日1978-09-19

    原文格式PDF

  • 申请/专利权人 DOW CHEMICAL COMPANY (THE);

    申请/专利号CA19750231907

  • 发明设计人 WALKER EDDIE B.;

    申请日0000-00-00

  • 分类号C08G59/04;C08G59/50;C08J3/00;

  • 国家 CA

  • 入库时间 2022-08-22 22:20:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号