首页> 外国专利> A method for the production of a magnetic or. Terms of its magnetizability adjustable sintered hard metal product

A method for the production of a magnetic or. Terms of its magnetizability adjustable sintered hard metal product

机译:一种生产磁性或磁性的方法。可磁化性可调的烧结硬质金属制品的术语

摘要

Sintered carbide prod. with opt. a magnetic or a non-magnetic binder matrix is produced by milling a mixt. of WC and Ti together with approx. 10% wt. Ni and sintering the compacted mixt. Sufficient Ti is added to form free W which then alloys with the Ni to form a binder matrix contg. is not 28% W. To form the non-ferromagnetic sintered carbide prod. the ratio of W in the binder to the binder alloy is 15-28% wt, whilst to form the ferromagnetic material this ratio is 14% wt. Pref. at least part of the Ti is added as a Ti-Ni alloy and/or Ti hydride. The compsn. may also contain approx. 1% wt Cr and grain growth during sintering is inhibited by adding 0.05-2.0% wt Ti. The props. can be made ferro-magnetic or non ferromagnetic as required whilst still retaining good strength and wear resistance together with chemical inertness. Used as magnetic type guides, cutting tools, and tools for glass making where Co contamination is detrimental.
机译:烧结碳化物产品。与选择。通过研磨混合物来制备磁性或非磁性粘合剂基质。 WC和Ti以及大约10%重量镍并烧结压实的混合物。加入足够的Ti以形成游离的W,然后将其与Ni合金化以形成粘合剂基质。不大于28%W。形成非铁磁烧结碳化物产品。粘结剂中的W与粘结剂合金的重量比为15-28%(重量),而形成铁磁材料时该重量比为14%(重量)。首选至少部分的Ti以Ti-Ni合金和/或氢化钛的形式添加。该compsn。可能还包含约。通过添加0.05-2.0%wt的Ti,可抑制1%wt的Cr和烧结过程中的晶粒长大。道具。可以根据需要制成铁磁或非铁磁,同时仍保持良好的强度和耐磨性以及化学惰性。用作磁性类型的导向器,切割工具和对Co有害的玻璃制造工具。

著录项

  • 公开/公告号DE2534919B2

    专利类型

  • 公开/公告日1977-12-22

    原文格式PDF

  • 申请/专利权人

    申请/专利号DE19752534919

  • 发明设计人

    申请日1975-08-05

  • 分类号C22C1/05;C22C29/00;

  • 国家 DE

  • 入库时间 2022-08-22 22:03:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号