1385429 Vulcanizable elastomer mixtures CHEMISCHE WERKE HULS AG 22 June 1972 [24 June 1971] 29241/72 Headings C3P and C3Q Vulcanizable mixtures comprise (1) an elastomer and (2) 2 to 20% by weight of the elastomer of polyoctenamer and/or polydodecenamer in which the proportion of double bonds in the transconfiguration is greater than 60%. Preferred polyalkenamers have a reduced specific viscosity of 0À2 to 3À0 dl./g. in decalin at 135‹ C. and a trans content of 75 to 95%. The elastomer may be natural rubber, polyisoprene, a butadiene polymer or copolymer, e.g. with styrene or acrylonitrile, polychloroprene, or an olefin copolymer or olefin/diene terpolymer rubber. In examples polyoctenamer and polydodecenamer are compounded with natural rubber, polyisoprene, SBR or polybutadiene in the presence of carbon black, aromatic plasticizer oil, zinc oxide, stearic acid and vulcanizing ingredients, and the compositions vulcanized.
机译:1385429可硫化的弹性体混合物CHEMISCHE WERKE HULS AG 1972年6月22日[1971年6月24日] 29241/72标题C3P和C3Q可硫化的混合物包含(1)弹性体和(2)重量比为20%的聚辛烯单体和/或聚十二烯单体的弹性体其中双键在反式构型中的比例大于60%。优选的聚烯烃具有降低的比粘度为0-2至3-0dl./g。在135℃下萘烷中的α-丁内酯和75-95%的反式含量。弹性体可以是天然橡胶,聚异戊二烯,丁二烯聚合物或共聚物,例如聚乙烯。与苯乙烯或丙烯腈,聚氯丁二烯或烯烃共聚物或烯烃/二烯三元共聚物橡胶。在实施例中,将聚辛烯和聚十二烯与天然橡胶,聚异戊二烯,SBR或聚丁二烯在炭黑,芳族增塑剂油,氧化锌,硬脂酸和硫化成分的存在下混合,并将组合物硫化。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号