Bituminous compsns. for filing expansion gaps and joints in road surfaces are produced by first mixing 20-45 wt. % of ground rubber and 55-80 wt. % of a petroleum oil fraction or extract at 20-100 r.p.m. and 25-120 degrees C for 1-3 hr. The mixt. (100 pts. wt.) is then stirred for 30 min. while adding 25-50 pts. wt. of spent oil shale and/or cement, and then mixed with 150-250 pts. wt. of preheated (160-180 degrees C) cold-resisting blown bitumen for 1-3 hr. Premixing (swelling) the rubber with petroleum oil improves the properties of the compsn., giving elastic products with a broad plastic temp. range and good adhesion to metals, concrete and asphalt. The products can be used as a ready-made strip or as a hot-pourable mass.
机译:沥青成分。用于填充膨胀缝隙和道路表面的接缝的方法是先混合20-45 wt。百分比的地面橡胶和55-80 wt。 20-100 r.p.m.的石油馏分或提取物的%。在25-120摄氏度下加热1-3小时。混音。然后将(100重量%)(30重量%)搅拌30分钟。同时增加25-50点。重量废油页岩和/或水泥,然后与150-250点混合。重量的预热(160-180摄氏度)耐寒吹制沥青1-3小时。将橡胶与石油进行预混(溶胀)可改善复合材料的性能,从而使弹性产品具有较宽的塑性温度。范围和对金属,混凝土和沥青的良好附着力。该产品可用作现成的条状或可热浇注的物料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号