机译:具有疏水性的高压灭菌低重量强度加气混凝土的生产方法

摘要

A method in the manufacture of steam-cured light-weight aerated concrete having hydrophobic properties, comprising preparing an aqueous expandable and solidifiable slurry, one or more hydraulic binders and one or more silica-containing materials casting the slurry in a mould; expanding and solidifying, and optionally cutting the solidified slurry; and steam-curing the resultant light-weight aerated concrete, wherein prior to casting said slurry it is admixed with silicone oil in a quantity of 0.05-0.50%, calculated on the dry weight of the starting mixture.
机译:一种具有疏水性的蒸汽固化的轻质加气混凝土的制造方法,该方法包括制备水性可膨胀和可固化的浆料,一种或多种水硬性粘合剂以及一种或多种将所述浆料浇铸在模具中的含二氧化硅的材料。膨胀和固化,并可选地切割固化的浆料;蒸汽固化所得的轻质加气混凝土,其中在浇铸所述浆料之前,将其与硅油混合,其量为起始混合物干重的0.05-0.50%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号