Method of preparation by hydrometallurgical of anhydride, molybdic of technical quality from 13 of molybdenite

机译:用湿法冶金从13钼矿中制取技术品质为钼的钼的方法

摘要

An improved hydrometallurgical method is provided for producing technical grade molybdic oxide from molybdenite concentrates. According to this method, the molybdenite concentrates are leached in an acid medium having a nitric acid concentration between about 25 gpl and about 50 gpl and an initial sulphuric acid concentration of nil to about 750 gpl, under oxygen pressure of about 100 - 250 psig and at a temperature above 115 DEG C so as to produce technical grade molybdic oxide having not more than 0.1% sulphur. Then a liquid-solid separation of the reaction mixture is effected and the obtained leach liquor is recycled back to the leaching stage optionally after partial neutralization with a basic reagent. The solid is washed and recovered as technical grade molybdic oxide.
机译:提供了一种改进的湿法冶金方法,用于从辉钼矿精矿生产工业级氧化钼。根据该方法,在约100-250 psig的氧气压力下和在约25 gpl至约50 gpl的硝酸浓度和零至约750 gpl的初始硫酸浓度的酸性介质中浸出辉钼矿精矿。在高于115℃的温度下生产出硫含量不超过0.1%的工业级氧化钼。然后进行反应混合物的液-固分离,并且任选地在用碱性试剂中和之后,将获得的浸出液再循环回到浸出阶段。洗涤固体并回收为工业级氧化钼。

著录项

  • 公开/公告号FR2330648B1

    专利类型

  • 公开/公告日1980-02-08

    原文格式PDF

  • 申请/专利权人 NORANDA MINES LTD;

    申请/专利号FR19750031718

  • 发明设计人

    申请日1975-10-16

  • 分类号C01G39/00;C22B3/00;

  • 国家 FR

  • 入库时间 2022-08-22 17:25:30