Size composition and method of producing same to render glass fiber having improved dispersibility in aqueous solutions
Size composition and method of producing same to render glass fiber having improved dispersibility in aqueous solutions
展开▼
机译:胶料组合物及其生产方法,以使玻璃纤维在水溶液中的分散性得到改善
展开▼
页面导航
摘要
著录项
相似文献
摘要
A sized composition and method of making same is provided for rendering sized glass fibers that have improved dispersibility in aqueous solutions. The size composition has about 35 to about 90 weight percent of the polyvinyl alcohol; and about 3 to about 14 weight percent of a polyamino functional polyamide resin; and about 1 to about 4 weight percent of an organic carboxylic acid having 1 to 5 carbon atoms, which is used to react with the polyamino functional polyamide resin to produce the carboxylic acid salt of the polyamino functional polyamide resin, wherein the amount of polyvinyl alcohol is at least about 5 times the amount of polyamide resin; and about 1 to about 10 weight percent of a nonionic wetting agent; about 0.5 to about 3 weight percent of an amino- alkyl-alkoxy-silane and about 5 to about 30 weight percent of an alkyl imidazoline textile softener. These weight percents are based on the non- aqueous components in the aqueous size solution. Also a anti-foaming agent may be incorporated into the size composition in an amount of about 0.1 to about 1 weight percent.
展开▼