首页> 外国专利> Manufacturing method of Carbon Steel or Low Alloy Steel during Refining, where the surface of the Melt is Pneumatic controlled temperature

Manufacturing method of Carbon Steel or Low Alloy Steel during Refining, where the surface of the Melt is Pneumatic controlled temperature

机译:熔体表面为气动控制温度的精炼过程中碳钢或低合金钢的制造方法

摘要

The method enables the desired tap temperature to be obtained during subsurface pneumatic refining of carbon steel or low alloy steel, without the need to reblow the heat, by adding to the melt, before starting the injection of refining oxygen, a fast oxidizing element such as aluminum, and a slow oxidizing element, such as silicon. The amount of fast oxidizing element added is such that the total amount thereof in the melt is sufficient, when oxidized, to raise the temperature of the melt to the desired temperature before substantial decarburization begins, and the amount of slow oxidizing element added is such that the total amount thereof is sufficient, when oxidized, to maintain the temperature of the melt within the desired temperature range during the decarburization period.
机译:该方法通过在开始注入精炼氧气之前向熔体中添加快速氧化元素,例如在碳精钢或低合金钢的地下气动精炼过程中,无需再吹热即可获得所需的出钢温度。铝和慢氧化元素,例如硅。所添加的快速氧化元素的量应足以使其在熔体中的总量在被氧化时足以在开始实质脱碳之前将熔体的温度升至所需温度,而所添加的缓慢氧化元素的量应使得当氧化时,其总量足以在脱碳期间将熔体的温度保持在所需的温度范围内。

著录项

  • 公开/公告号AR221618A1

    专利类型

  • 公开/公告日1981-02-27

    原文格式PDF

  • 申请/专利权人 UNION CARBIDE CORP;

    申请/专利号AR19790277825

  • 发明设计人

    申请日1979-08-23

  • 分类号C21C5/00;

  • 国家 AR