A finely-ground nickel-copper matte is leached using an acid at a minimum temperature of approx. 80 DEG C. and under oxidizing conditions in order to produce a nickel sulfate solution and a nickel-cooper sulfide residue, which is separated from the solution and thereafter the nickel-copper sulfide residue is leached using acid in an autoclave at a minimum temperature of 110 DEG C. and under oxidizing conditions in order to produce an additional quantity of nickel sulfate solution and a copper sulfide precipitate.
机译:使用酸在最低约25°F的高温下浸出细磨的镍铜哑光粉。为了产生硫酸镍溶液和从溶液中分离出的镍-铜-硫化铜残留物,在80℃和氧化条件下,然后在最低温度为80℃的高压釜中用酸浸出镍-铜-硫化铜残留物。为了产生额外量的硫酸镍溶液和硫化铜沉淀,在110℃和氧化条件下进行。

著录项

  • 公开/公告号BR8004019A

    专利类型

  • 公开/公告日1981-01-21

    原文格式PDF

  • 申请/专利权人 OUTOKUMPU OY;

    申请/专利号BR19808004019

  • 发明设计人 MATTI SEILO;HEIMO UNTO AUGUST SAARINEN;

    申请日1980-06-26

  • 分类号C22B3/00;C22B15/08;

  • 国家 BR

  • 入库时间 2022-08-22 16:19:28

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号