Low rank coal is dewatered and upgraded by heating a coal/water mixture at 150° to 300° C. at a pressure preventing water vaporization, mechanically separating the water, then heating the coal at 300° to 400° C. at a pressure allowing water vaporization.
机译:通过在防止水汽化的压力下将煤/水混合物在150°C至300°C加热,机械分离水,然后在300°C至400°C的压力下加热煤来对低级煤进行脱水和提质。水汽化。