The process of the invention is for the separate recovery of elemental sulfur and residual sulfides and metal salt solution from reaction slurries obtained from leaching of metal sulfides in ores and concentrates. The process comprises directing flow of a said reaction slurry at a temperature at which sulfur is present in the liquid state and at a pressure such that flashing of vapor is avoided into a separating step comprising a substantially quiescent zone, coalescing said elemental sulfur in the substantially quiescent zone, settling coalesced sulfur together with unreacted sulfides from said quiescent zone, maintaining a velocity in said flow in said substantially quiescent zone to cause separation of said slurry into a first and a second fraction, said velocity having an upward velocity component, said first fraction containing dissolved metals and at least one material chosen from gangue materials and precipitated compounds, said at least one material having a terminal settling velocity less than said upward velocity component, and said second fraction containing coalesced liquid elemental sulfur and unreacted sulfides, and separately discharging said first and second fractions from said separating step.
机译:本发明的方法是从矿石和精矿中浸出金属硫化物得到的反应浆料中分别回收元素硫和残留的硫化物以及金属盐溶液。该方法包括将所述反应淤浆在一定温度下引导流动,所述温度下硫以液态存在并且处于一定压力下,从而避免蒸气闪蒸进入包括基本静止区的分离步骤,在所述基本静止区中合并所述元素硫。静态区,将聚结的硫与未反应的硫化物一起沉降到所述静态区中,在所述基本静态区中保持所述流中的速度,以使所述浆料分离为第一和第二部分,所述速度具有向上的速度分量,所述第一包含溶解的金属和至少一种选自石材料和沉淀化合物的材料的馏分,所述至少一种材料的最终沉降速度小于所述向上的速度分量,所述第二馏分包含聚结的液态元素硫和未反应的硫化物,并分别排放所述s的第一和第二部分分离步骤。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号