process for the recovery of potassium jarositul, so3, fe2o3 and k2so4 as or converted in na2so4 and koh, according to the invention, consists in that jarositul potassium,it is subjected to thermal decomposition at a temperature of approximately 1000 degree c for 1h.on the one hand so3 valorificabil resulting form of h2so4 and, on the other hand, a solid mixture consisting of feo3 and k2so4 from which further by washingdrying and macinare can be harnessed in pigmentilor industry or for obtinereafierului soft and k2so4 solution which form by concentration and crystallization can be harnessed as such tothey can be of k2so4 solution over a resin ion exchange last average prominent brow points to a male form ohwhen is it holding anionului so4laputerea 2 - and training in effluent of koh which can be used to getting jarositului potassium,rasinii and regeneration with a solution of naoh to form a solution of na2so4 which can be harnessed by crystallization.
机译:根据本发明的用于回收作为或在Na 2 SO 4和酸中转化的钾,钾,SO 3,Fe 2 O 3和K 2 SO 4的方法的方法在于,在约1000℃的温度下对其进行热分解1小时。一方面是h2so4的发价形式,另一方面是由feo3和k2so4组成的固体混合物,可以进一步通过洗涤干燥和Macinare从中得到利用,用于颜料色浆工业,或者用于浓缩和结晶形成的obretreafierului软和k2so4溶液。可以利用它们在树脂离子交换上的k2so4溶液中最后一个显着的眉头指向雄性形式,何时它持有anionului so4laputerea 2-并在koh废水中进行培训,以用于获得jarositului钾,rasinii和用Naoh溶液再生以形成Na2so4溶液,可通过结晶加以利用。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号