This invention relates to the making process of steel plate having impact toughness. The steel plate contains=0.15% Carbon, =1.0% Silicon, 1.0- 0.2% Manganese, 0.01 - 0.08% niobium, =0.10% Vanadium, =0.4% molybdenum, =0.4% nickel, 0.01- 0.03% titanium. The steel plate is rolled at the temperature of 850 - 750 ≦̸C. And then, the steel plate is cooled by the water injection. So the cooling speed is 5 - 20≦̸C/sec, and the temperature is 650 - 550≦̸C.
机译:本发明涉及具有冲击韧性的钢板的制造方法。钢板包含> = 0.15%碳,> = 1.0%硅,1.0- 0.2%锰,0.01- 0.08%铌,> = 0.10%钒,> = 0.4%钼,> = 0.4%镍,0.01- 0.03%钛。钢板在850-750℃的温度下轧制。然后,通过注水将钢板冷却。因此,冷却速度为5-20°C /秒,温度为650-550°C。

著录项

  • 公开/公告号KR830000483A

    专利类型

  • 公开/公告日1983-03-10

    原文格式PDF

  • 申请/专利权人 POHANG IRON & STEEL CO LTD;

    申请/专利号KR19810002636

  • 发明设计人 KIM TAE WUNG;

    申请日1981-07-21

  • 分类号C21C5/00;

  • 国家 KR

  • 入库时间 2022-08-22 10:27:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号