首页> 外国专利> METHOD FOR DEPHOSPHORIZING MOLTEN IRON BY BLOWING SLAG FORMING AGENT INTO MOLTEN IRON BATH

METHOD FOR DEPHOSPHORIZING MOLTEN IRON BY BLOWING SLAG FORMING AGENT INTO MOLTEN IRON BATH

机译:通过将渣SL形成剂吹入熔融铁浴中使熔融铁脱磷的方法

摘要

PURPOSE:To dephosphorize effectively molten iron by blowing only a slag forming agent for dephosphorization into the molten iron at a specified depth from the surface of the molten iron bath through a lance with an inert gas and by adding an oxidizing agent to the surface of the bath at the same time. CONSTITUTION:A slag forming agent 7 for dephosphorization is blown into molten iron 2 in a molten iron ladle 1 at =500mm. depth from the surface of the molten iron bath through a lance 4 with an inert gas 6 as a carrier gas. At the same time, an auxiliary slag forming agent 9 and an oxidizing agent 8 are added to the surface of the bath. The granules of the blown slag forming agent 7 diffuse in the molten iron 2 and rise to the surface of the bath while being heated. The granules become an active state and react efficiently with P2O5 formed by the reaction of the oxidizing agent 8 with phosphorus in the molten iron 2. The P2O5 is fixed in slag 3.
机译:用途:有效地对铁水进行脱磷的方法是,仅用惰性气体通过喷枪将规定的脱磷炉渣形成剂从铁水熔池表面吹入规定深度的指定深度,然后将氧化剂添加到铁水中。在同一时间洗澡。组成:用于脱磷的炉渣形成剂7在> = 500mm的温度下吹入铁水包1中的铁水2中。从钢水熔池的表面到通过喷枪4的深度,以惰性气体6作为载气。同时,将辅助炉渣形成剂9和氧化剂8添加到熔池的表面。吹渣形成剂7的颗粒在铁水2中扩散并在加热的同时上升到熔池的表面。颗粒变为活性状态并与由氧化剂8与铁水2中的磷反应形成的P2O5有效地反应。P2O5固定在炉渣3中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号