PURPOSE:To obtain the titled low-cost steel plate producing no stretcher strain even in a multi-step drawing stage by providing a specified composition consisting of C, Si, Mn, Cr, N, Fe and inevitable impurities and having specified relation. CONSTITUTION:A ferritic stainless steel plate producing no stretcher strain is obtd. by providing a composition consisting of, by weight, =0.08% C, =0.70% Si, =1.00% Mn, 15-20% Cr, 0.04-0.12% N (C+N=0.08-0.15%) and the balance Fe with inevitable impurities. 0.08% C deteriorates the corrosion resistance and toughness and hardens the material. 0.70% Si hardens the material and reduces the elongtion. 1.00% Mn hardens the material. 15% Cr does not give the desired corrosion resistance, and 20% Cr makes looping remarkable. N and C+N prevent the production of a stretcher strain in said ranges, yet more than the uppr limits of N and C+N harden the material.
机译:目的:通过提供由C,Si,Mn,Cr,N,Fe和不可避免的杂质组成的指定组成并具有指定关系,来获得即使在多步拉伸阶段也不会产生拉伸应变的标题低成本钢板。组成:铁素体不锈钢板不会产生拉伸应变。通过提供按重量计由<= 0.08%C,<= 0.70%Si,<= 1.00%Mn,15-20%Cr,0.04-0.12%N(C + N = 0.08-0.15%)和其余的铁中不可避免地带有杂质。 > 0.08%C会使耐腐蚀性和韧性变差,并使材料变硬。 > 0.70%Si会硬化材料并降低延伸率。 Mn> 1.00%会使材料硬化。 Cr小于15%不能提供所需的耐腐蚀性,Cr大于20%会使循环显着。 N和C + N阻止在上述范围内产生拉伸应变,但超过N和C + N的最高极限会使材料硬化。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号