首页>
外国专利>
LEAD ALLOY ANODE FOR ELECTROWINNING OF ZINC
LEAD ALLOY ANODE FOR ELECTROWINNING OF ZINC
展开▼
机译:锌电解镀铅合金阳极
展开▼
页面导航
摘要
著录项
相似文献
摘要
A lead alloy anode for a cell for the electrowinning or electrolytic recovery of zinc consists of 0.05 to 0.25% by weight strontium and/or 0.05 to 0.1% by calcium in combination with 0.1 to 0.5 silver, balance lead. The cell is used in a method for the recovery of zinc at, for example, a current density of 160 to 630 amp/m2, a temperature of 30 DEG to 46 DEG C. and an electrolyte containing 40 to 70 g/l zinc and 165 to 220 g/l sulfuric acid.
展开▼
机译:用于锌的电解沉积或电解回收的电池的铅合金阳极由0.05至0.25%的锶和/或0.05至0.1%的钙以及0.1至0.5的银组成。该电池用于例如在160至630amp / m 2的电流密度,30至46℃的温度和包含40至70g / l的锌和165至220 g / l硫酸。
展开▼