PURPOSE:To produce a rolling roll having the special shape and service characteristics requiring strength and toughness in the neck end part thereof by forming the cylindrical shell part, cylindrical core part, bearing part and neck end part of said roll of specific materials. CONSTITUTION:The titled method relates with a special rolling roll which has the slender neck shape of 0.8-1.2lN/lB ratio between neck length and body length of 3.8-13.0lN/DN ratio between neck length and neck diameter and in the neck end part of which large stress is generated. The cylindrical shell part 1a thereof is formed of an adamite material or alloy cast iron material; on the other hand, the cylindrical core part 1b and bearing part 2 are formed of a spheroidal graphite cast iron material having 40-50 hardness HS, 40-55kg/ mm.2 tensile strength and 0.5-1.5% elongation. One or both of the neck end parts 3 are formed of a steel material having 30-45 hardness HS, 55kg/mm.2 tensile strength and =1.5% elongation. The three parts mentioned above are welded by fusion to one body.
机译:用途:通过形成所述特定材料的所述辊的圆柱壳部,圆柱芯部,轴承部和颈部端部,来制造具有特殊形状和使用特性的轧辊,所述特殊形状和使用特性需要在其颈部端部具有强度和韧性。组成:该标题方法涉及一种特殊的轧辊,该轧辊的细长颈部形状在颈部长度与体长之比为0.8-1.2lN / lB,在颈部长度与颈部直径之和在颈部末端为3.8-13.0lN / DN会产生很大的应力。其圆筒形壳体部分1a由金刚砂材料或合金铸铁材料形成;另一方面,圆筒形芯部1b和轴承部2由具有40-50硬度HS,40-55kg / mm 2的抗拉强度和0.5-1.5%的伸长率的球墨铸铁材料形成。颈部末端部分3中的一个或两个由具有30-45的硬度HS,55kg / mm 2的抗张强度和≥1.5%的伸长率的钢材形成。上面提到的三个部分通过熔合焊接到一个主体上。

著录项

  • 公开/公告号JPS6018484B2

    专利类型

  • 公开/公告日1985-05-10

    原文格式PDF

  • 申请/专利权人 KUBOTA LTD;

    申请/专利号JP19820069133

  • 申请日1982-04-23

  • 分类号B22D19/16;B21B27/00;B21B27/02;B21B27/03;C22C37/00;

  • 国家 JP

  • 入库时间 2022-08-22 08:34:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号