A method is provided for leaching comminuted nickeliferous sulfide matte containing by weight about 20 to 75% nickel, about 5 to 50% copper, non-stoichiometric sulfur in the range of over 4 to about 24%, over 0.5 to about 20% iron, the sum of the nickel, copper and sulfur contents being at least about 80% of the matte composition, with the balance gangue or slag and incidental impurities.