Procedure for Toughening unsaturated Polyester Resins.
Procedure for Toughening unsaturated Polyester Resins.
展开▼
机译:增韧不饱和聚酯树脂的程序。
展开▼
页面导航
摘要
著录项
相似文献
摘要
Process for the production of unsaturated Polyester Resins Accelerated.Is to react - 75 30 parts by weight of ethylenically unsaturated Polyester Ba, BB -, 70 - 25 parts by weight of monomers with the previous copolimerizables with 1.0 - 10 weight, referred to the unsaturated Polyester resin, Accelerator of formula (i) and other Auxiliary agents under dist Ribucion Homogeneous and thus obtained the Mass Hardens where R1 and R2 are a remnant HydrocarbonSaturated or unsaturated with C 1 to 18; R3 and R4 are a remaining alkyl C 1 to 4 and others.
展开▼
机译:加速反应的不饱和聚酯树脂的生产方法-75-30 30重量份的烯键式不饱和聚酯Ba,BB-,70-25重量份的单体与先前的可共聚合的1.0-10重量份,称为不饱和聚酯树脂,式(i)的促进剂和其他助剂在均匀分布下得到,因此得到了质量硬化,其中R 1和R 2为残余的烃,其饱和或不饱和的碳原子数为1至18; R 3和R 4为剩余的烷基C 1至4等。