COAL-WATER FUEL SLURRY AND A PROCESS FOR ITS PREPARATION

机译:水煤浆及其制备方法

摘要

Coal-water fuel slurries having long-term storage stability and improved viscosities and comprising finely-divided coal having a particle size distribution which is 100% -50 mesh (-297 mu ) and at least 50% -200 mesh (-74 mu ) said coal being in an amount sufficient to provide a suitable coal concentration in the slurry so as to remain within efficient combustion size range, water, and minor amounts of alkali metal salts of organic dispersants to reduce the viscosity of the slurry and alkaline earth metal salts of organic dispersants to obtain a higher slurry yield point and provide a substantially stable static dispersion and a process for making such slurries.
机译:具有长期存储稳定性和改善的粘度并且包含粒度分布为100%-50目(-297 mu)和至少50%-200目(-74 mu)的细碎煤的水煤浆所述煤的量足以在浆料中提供合适的煤浓度,以保持在有效燃烧尺寸范围内,水和少量有机分散剂的碱金属盐以降低浆料和碱土金属盐的粘度制备有机分散剂以获得更高的浆料屈服点并提供基本稳定的静态分散体和制备这种浆料的方法。

著录项

  • 公开/公告号NZ203626A

    专利类型

  • 公开/公告日1986-02-21

    原文格式PDF

  • 申请/专利权人 ATLANTIC RESEARCH CORP.;

    申请/专利号NZ19830203626

  • 发明设计人 SCHEFFEE R.S.;

    申请日1983-03-18

  • 分类号C10L1/32;

  • 国家 NZ

  • 入库时间 2022-08-22 07:40:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号