首页> 外国专利> Textile finishing agent - contg. nonionic surfactant obtd. by adding alkylene oxide to amine cpd. obtd. by condensing fatty acid with poly:alkylene poly:amine

Textile finishing agent - contg. nonionic surfactant obtd. by adding alkylene oxide to amine cpd. obtd. by condensing fatty acid with poly:alkylene poly:amine

机译:纺织品整理剂-续非离子表面活性剂通过将氧化烯加成到胺cpd上。 t。通过将脂肪酸与聚:亚烷基聚:胺缩合

摘要

The finishing agent contains 0.5-10 (1-10) wt. % of nonionic surfactant prepd. by adding 1-50 (3-30) mol. of alkylene oxide to1 mol. of an amide cpd. obtd. by dehydration condensn. of 8-24C higher fatty acid and polyalkylene polyamine of formula H2N(-(CH2)n-NH)mH(I) (where n is 1 to 3; m is 2 to 9). Pref. higher fatty acids are stearic and behenic acids. The polyalkylene polyamine includes diethylene triamine, triethylene tetramine, tetramethylene pentamine, etc. The fatty acid and polyalkylene polyamine are used in a molar ratio of 3:1 to 1:1. The alkylene oxide is ethylene oxide or its mixt. with propylene oxide with an ethylene oxide content of at least 50 wt. %. The finishing agent contains 1-30 wt.% of lubricant.
机译:整理剂包含0.5-10(1-10)重量%。非离子表面活性剂的制备百分比。通过添加1-50(3-30)mol。环氧烷至1摩尔。酰胺的cpd。 obtd。通过脱水冷凝。 8-24℃的高级脂肪酸和式H 2 N(-(CH 2)n -NH)m H(I)的聚亚烷基多胺(其中n为1至3; m为2至9)。首选高级脂肪酸是硬脂酸和山hen酸。聚亚烷基多胺包括二亚乙基三胺,三亚乙基四胺,四亚甲基五胺等。脂肪酸和聚亚烷基多胺的摩尔比为3∶1至1∶1。环氧烷是环氧乙烷或其混合物。环氧乙烷的含量至少为50 wt。 %。整理剂包含1-30重量%的润滑剂。

著录项

  • 公开/公告号ES8603603A1

    专利类型

  • 公开/公告日1985-12-16

    原文格式PDF

  • 申请/专利权人 KAO CORPORATION;

    申请/专利号ES19840537188

  • 发明设计人

    申请日1984-10-29

  • 分类号D06M13/38;

  • 国家 ES

  • 入库时间 2022-08-22 07:37:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号