Activated ash cement containing Portland cement clinker in a proportion of 40 to 55 parts by weight, characterised in that it also contains gypsum dihydrate or phosphogypsum in a proportion of 1.5 to 5 parts by weight, ash originating from electrical filters of thermal power stations in a proportion of 35 to 55 parts by weight, and sodium-potassium silicate in a proportion of 0.5 to 2.0 parts by weight, monoethylene glycol in a proportion of 0.25 to 1.0 part by weight, sodium carbonate in a proportion of 0.2 to 0.8 part by weight, sodium nitrate in a proportion of 0.2 to 1.0 part by weight and added cement in a proportion of 3.0 to 6.0 parts by weight, which define a chemical additive.
机译:活性灰水泥中的硅酸盐水泥熟料含量为40至55重量份,其特征在于它还含有二水合石膏或磷石膏,其含量为1.5至5重量份,这些灰来自于火力发电厂的电力过滤器。 35至55重量份的硅酸钠,0.5至2.0重量份的硅酸钠钾,0.25至1.0重量份的单乙二醇,0.2至0.8重量份的碳酸钠,以0.2至1.0重量份的比例添加硝酸钠,并以3.0至6.0重量份的比例添加水泥,它们定义了化学添加剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号