According to the present invention, Ni- and Co-rich, low Mg fines may be advantageously separated from the coarse fractions of lateritic ores by atmospheric or low pressure leaching. In particular, the process of the present invention comprises contacting a lateritic ore or ore fraction at temperatures from about 20 DEG C. to about 200 DEG C. and pressures from about atmospheric to about 200 psig with an aqueous acid solution to form a leach liquor, a leach residue and a fines fraction. The fines fraction which can be separated from the residue with the leach liquor by conventional means such as cycloning is found to be richer in Ni and Co and lower than the remainder of the residue.
机译:根据本发明,可以通过大气压或低压浸出将富Ni和Co的低Mg细粉从红土矿石的粗级分中分离出来。特别地,本发明的方法包括使红土矿石或矿石级分在约20℃至约200℃的温度和约大气压至约200psig的压力下与酸性水溶液接触以形成浸出液。 ,浸出残渣和细粒级分。发现可以通过常规方法例如环化与浸出液从残余物中分离出的细粉部分富含Ni和Co,并且低于残余物的其余部分。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号