A FEEDER FOR SUPPLYING STREAMS OF HEAT SOFTENED MINERAL MATERIAL IN FILAMENT FORMING CONDITION FOR USE IN AN APPARATUS FOR ATTENUATING HEAT-SOFTENED MINERAL MATERIALS AND APPARATUS HAVING SAID FEEDER

机译:供给供热软化矿物材料的流水线的供料器,供成丝条件用于用于减弱具有供料器的热化矿物材料和设备的设备

摘要

A glass fiber attenuation apparatus and process wherein molten glass is supplied from a molten glass body to an orifice plate at substantially atmospheric pressure to prevent molten glass flow through an orifice at which attenuation has ceased, thus permitting continuation of the attenuation process despite breakouts at individual orifices. The preferred embodiment of the method includes the steps of cooling the orifice plate undersurface to a non-wetting temperature and delivering molten glass to the orifice plate at a pressure less than the internal, surface tension-generated pressure of any bead formed on the undersurface of the orifice plate upon attenuation cessation at that orifice. The preferred embodiment of the apparatus includes a perforate pressure plate immersed in the body of molten glass and superimposed over the orifice plate to effect a pressure drop upon normal attenuation flow which is sufficient to reduce the pressure immediately above the orifice plate to substantially atmospheric pressure or, in any event, to a pressure less than the internal pressure of a bead or globule formed on attenuation cessation at an orifice. The orifice plate may be of either the planar, non-tipped type or of the tipped type, and the orifice plate may be cooled to the appropriate temperature either by gas flow cooling directed at the undersurface of the orifice plate or by fin shields.
机译:一种玻璃纤维衰减装置和方法,其中熔融玻璃在大气压下从熔融玻璃体供应到孔板,以防止熔融玻璃流过衰减已经停止的孔,因此尽管在单个处破裂,仍允许继续衰减过程。孔口。该方法的优选实施例包括以下步骤:将孔板下表面冷却至非润湿温度,并将熔融玻璃以小于形成在管子下表面上的任何珠的内部,表面张力产生的压力的压力输送至孔板。在该孔口处停止衰减后的孔口板。该设备的优选实施例包括浸入熔融玻璃体中并叠加在孔板上方的穿孔压力板,以在正常衰减流时产生压降,该压降足以将孔板上方的压力直接降低至基本为大气压或在任何情况下,压力要小于孔口衰减停止时形成的小珠或小球的内部压力。孔板可以是平面的,不倾斜的类型,也可以是倾斜的类型,并且可以通过导向孔板底面的气流冷却或通过翅片罩将孔板冷却至适当的温度。

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号