SLOW-DEFLAGRATING,NITROESTERIC MINING EXPLOSIVE WITH HIGH WATER-RESISTANT CHARACTERISTICS

机译:具有高耐水特性的慢碎片化,非平衡开采

摘要

Nitroesther deflagration resistant mining explosive with high water resistance, containing 80:20 mixture of nitro glycol and nitro-glycerine, and/or 20-30% by weight nitro glycol, 0.5-1.5% by weight nitrocellulose, 40-70% by weight ammonium nitrate, 4-10% by weight soda nitre, 3-10% by weight dinitrotoluene and/or trinitrotoluene and waterproofing agent including barium sulphate as a carrier; is characterised in that contains waterproofing additive with 1:6:2 mixture of dextrin, barium sulphate and slack wax, containing optimally from 0.2-1% by weight dextrin, 1.8% by weight barium sulphate with relevant surface 500-600 cm2/g and 0.2-2% per weight of slack wax.
机译:具有高耐水性的耐硝酸盐爆燃矿用炸药,包含80:20的硝酸乙二醇和硝化甘油的混合物和/或20-30%的硝酸乙二醇,0.5-1.5%的硝酸纤维素,40-70%的铵硝酸盐,4-10%(重量)的纯碱,3-10%(重量)的二硝基甲苯和/或三硝基甲苯以及包括硫酸钡作为载体的防水剂;其特征在于,其包含具有糊精,硫酸钡和疏松蜡的1:6:2混合物的防水添加剂,其最佳含有0.2-1重量%的糊精,1.8重量%的硫酸钡,其相关表面为500-600cm 2。 / g和0.2-2%(重量)的松散蜡。

著录项

  • 公开/公告号PL265706A2

    专利类型

  • 公开/公告日1988-06-09

    原文格式PDF

  • 申请/专利权人

    申请/专利号PL19870265706

  • 发明设计人

    申请日1987-05-15

  • 分类号C06B;

  • 国家 PL

  • 入库时间 2022-08-22 06:59:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号