PURPOSE:To improve various magnetic characteristics including permeability in a high-frequency range by containing ZrO2 enhancing working characteristics and CaO as a low loss material into a fundamental composition composed of Fe2O3, ZnO and MnO and comprising at least one kind of TiO2 and SnO2 improving magnetic characteristics such as permeability in the high-frequency range. CONSTITUTION:50-65mol% Fe2O3, 5-30mol% ZnO and 10-40mol% MnO are used as a fundamental composition, and 0.01-0.2wt.% ZrO2 and 0.01-0.5wt.% CaO are contained while at least one kind of TiO2 and SnO2 is included at 0.01-0.3wt.%. An effect remarkable for improving the magnetic loss characteristics of a ferrite material is obtained because ZrO2 is contained, and low magnetic loss is acquired by including CaO into the fundamental composition of the ferrite material. At least one kind of TiO2 and SnO2 is added because magnetic characteristics more excellent than the single addition of CaO are obtained owing to composition addition with CaO.
机译:用途:通过将ZrO2增强工作特性和CaO作为低损耗材料包含在由Fe2O3,ZnO和MnO组成并包含至少一种TiO2和SnO2改善成分的基本成分中,来改善包括高频导磁率在内的各种磁特性。磁特性,例如高频范围内的磁导率。组成:以50-65mol%的Fe2O3、5-30mol%的ZnO和10-40mol%的MnO为基本成分,并包含0.01-0.2wt。%的ZrO2和0.01-0.5wt。%的CaO,同时至少一种TiO 2和SnO 2的含量为0.01-0.3重量%。通过含有ZrO 2,可以得到提高铁氧体材料的磁损耗特性的显着效果,通过在铁氧体材料的基本组成中含有CaO,可以得到低的磁损耗。添加至少一种TiO 2和SnO 2的原因在于,由于通过添加CaO而获得了比一次添加CaO更优异的磁特性。

著录项

  • 公开/公告号JPH01129403A

    专利类型

  • 公开/公告日1989-05-22

    原文格式PDF

  • 申请/专利权人 SONY CORP;

    申请/专利号JP19870287510

  • 发明设计人 TAKAHASHI YOSHIMI;SASAKI NORIO;

    申请日1987-11-16

  • 分类号C04B35/38;H01F1/34;

  • 国家 JP

  • 入库时间 2022-08-22 06:47:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号