FORMATION OF CORROSION PREVENTING FILM WITHSTANDING ACIDIC ENVIRONMENT

机译:酸性环境下防腐膜的形成

摘要

PURPOSE:To form a corrosion preventing film withstanding an oxidizing environment on a surface to be treated, by pretreating the surface, thermally spraying a metal and ceramics in succession and carrying out pore sealing treatment. CONSTITUTION:A surface requiring anticorrosive treatment is pretreated by grit blasting to expose the base and Mo, Ni, Cu, Fe or a multicomponent alloy of such metals is thermally sprayed. A ceramic layer is then laminated by thermal spraying so as to inhibit oxidation at high temp. and a pore sealing agent is impregnated. Thus, a corrosion preventing film withstanding an oxidizing environment contg. hydrochloric acid, sulfuric acid, etc., is formed on the surface to be treated.
机译:目的:通过对表面进行预处理,依次对金属和陶瓷进行热喷涂并进行气孔密封处理,从而在要处理的表面上形成能承受氧化环境的腐蚀防护膜。组成:需要喷砂处理的表面需要进行防腐处理,以暴露出基材,然后热喷涂Mo,Ni,Cu,Fe或此类金属的多组分合金。然后通过热喷涂层压陶瓷层,以抑制高温下的氧化。并且浸渍有孔密封剂。因此,耐腐蚀膜可承受氧化环境。在要处理的表面上形成盐酸,硫酸等。

著录项

  • 公开/公告号JPS6425960A

    专利类型

  • 公开/公告日1989-01-27

    原文格式PDF

  • 申请/专利权人 KANMETA ENG KK;

    申请/专利号JP19870181392

  • 发明设计人 UENO GUNJI;ISHIKAWA KAZUO;

    申请日1987-07-21

  • 分类号C23C4/02;C23C4/06;C23C4/18;

  • 国家 JP

  • 入库时间 2022-08-22 06:44:59

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号