AbstractThe pozzolanic properties of a pozzolanic material,more particularly a fly ash, are improved by mixing thepozzolanic material with a calciumoxyde or calciumhydroxidecontaining material and water in such a way that at thetime of associating or bringing together the abovementionedcomponents the mixture has or immediately attains a tempera-ture of more than 50°C, preferably at least 80°C, mostpreferably 85 to 100°C.A mixture of pozzolanic material and calciumoxydeand/or calciumhydroxide may be preheated, subsequently,water being added to said mixture.Water as used may be hot water and said water ispreferably added as one mass at one moment.The pozzolanic material obtained from the processof the invention is suitable as cement substitute, asmaterial for manufacturing building articles and a binderfor occluding one or more fillers to be introduced into achemical process or one or more fillers presenting noxiousproperties.
机译:抽象火山灰材料的火山灰性质,特别是粉煤灰,通过混合带有氧化钙或氢氧化钙的火山灰材料含有物质和水的方式关联或集合上述内容的时间混合物具有或立即达到温度的成分最高温度超过50°C,最好至少80°C优选85至100℃。火山灰材料和氧化钙的混合物和/或氢氧化钙可以预先加热,将水加入到所述混合物中。使用的水可以是热水,而所说的水是最好一次加入一团。从该方法获得的火山灰材料本发明的化合物适合用作水泥替代品,因为用于制造建筑制品的材料和粘合剂用于阻塞一种或多种填充剂化学过程或一种或多种有毒的填料属性。

著录项

  • 公开/公告号CA1250326A

    专利类型

  • 公开/公告日1989-02-21

    原文格式PDF

  • 申请/专利权人 AARDELITE HOLDING B.V.;

    申请/专利号CA19860507079

  • 发明设计人 LOGGERS HENDRIK;

    申请日1986-04-18

  • 分类号C04B11/26;

  • 国家 CA

  • 入库时间 2022-08-22 06:36:29

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号