LEACHING METHOD OF NI FROM THE LOW FINENESS ORE

机译:低品位矿中NI的浸出方法

摘要

Extraction of nickel from the low quality laterite ore is effected by leaching electrochemically in the electrolysis bath with a separator between cathod chamber and anode chamber. Nickel is recovered from 0.01-10.0 mol. sulfuric acid solution with blowing the sulfurous acid gas. Also anode chamber consists of 0.01-10.0 mol. sulfuric acid solution including source ore powder under 10 mesh.
机译:通过在电解槽中使用阴极室和阳极室之间的隔板进行电化学浸出,可以从劣质红土矿石中提取镍。从0.01-10.0摩尔回收镍。用硫酸溶液吹入亚硫酸气体。阳极室也由0.01-10.0mol组成。硫酸溶液包括10目以下的原矿粉。