首页> 外国专利> Method for bonding and/or repairing component parts made of an oxide dispersion-hardened nickel-based superalloy in the zone-annealed state of coarse-grained, longitudinally oriented column crystals

Method for bonding and/or repairing component parts made of an oxide dispersion-hardened nickel-based superalloy in the zone-annealed state of coarse-grained, longitudinally oriented column crystals

机译:在粗晶粒纵向取向的柱状晶体的区域退火状态下,结合和/或修复由氧化物弥散硬化的镍基高温合金制成的零件的方法

摘要

Component parts made of an oxide dispersion-hardened nickel-based superalloy in the state of coarse-grained, longitudinally oriented column crystals are renovated by fusion welding according to the argonarc, electron-beam, laser-beam or plasma-burner method by build-up welding (deposition welding, overlay welding) and/or joined together by junction welding, by first being subjected to a heat treatment in order to increase their ductility. Said heat treatment comprises solutionisation in the temperature range between 1160@C and 1280@C, followed by slow cooling at a rate of from 0.1@C/min to 5@C/min, to a temperature in the range between 500@C and 700@C, followed by cooling in air down to room temperature. Particularly advantageous economical method for in situ repairs on guide vanes (diffuser blades) and rotor blades of gas turbines. IMAGE
机译:由氧化物弥散硬化的镍基高温合金制成的粗颗粒,纵向取向的柱状晶体组成的零件,通过氩弧焊,电子束,激光束或等离子燃烧器的方法,通过熔焊进行修整,其结构如下:首先进行热处理以增加其延展性,然后进行向上焊接(沉积焊,堆焊)和/或通过接合焊连接在一起。所述热处理包括在1160℃至1280℃之间的温度范围内固溶,然后以0.1℃/ min至5℃/ min的速率缓慢冷却至500℃至250℃之间的温度。 700 @ C,然后在空气中冷却至室温。用于在燃气轮机的导向叶片(扩散叶片)和转子叶片上进行现场修复的特别有利的经济方法。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号