Method of preparing an aluminum oxide containing quartz glass activated by bivalent europium and comprising as glass matrix oxides mainly SiO.sub.2 and furthermore per mol of SiO.sub.2 up to at most 0.15 mol of at least one of the oxides, Al.sub.2 O.sub.3, B.sub.2 O.sub.3, P. sub.2 O.sub.5, ZrO.sub.2, Scf.sub.2 O.sub.3, Y.sub.2 O.sub.3, La.sub.2 O. sub.3, Gd.sub.2 O.sub.3, Lu.sub.2 O.sub.3, the alkali metal oxides and the alkaline earth metal oxides. A mixture is made of the composite oxides or of compounds which yield these oxides. The mixture comprises europium in the form of an aluminum containing compound of bivalent europium. The mixture is melted at a high temperature in a reducing atmosphere and is then cooled. The luminescent quartz glasses obtained are used in luminescent screens of, for example, low-pressure mercury vapor discharge lamps.
机译:制备含有被二价euro活化的石英玻璃的氧化铝的方法,该氧化铝包含主要为SiO 2的氧化物和作为玻璃基质的氧化物,此外每摩尔SiO 2最多至多0.15 mol的至少一种氧化物Al O.sub.2 O.3,B.sub.2 O.3,P.sub.2 O.sub.5,ZrO.sub.2,Scf.sub.2 O.sub.3,Y 2 O 3,La 2 O 3,G 2 O 3,Lu 2 O 3,碱金属氧化物和碱土金属氧化物。由复合氧化物或产生这些氧化物的化合物制成混合物。该混合物包含二价euro的含铝化合物形式的euro。将混合物在还原气氛中在高温下熔融,然后冷却。所获得的发光石英玻璃用于例如低压汞蒸气放电灯的发光屏。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号