A process of preparing a homogeneous amorphous polymeric blend of polyethyleneterephthalate (PET) and polybutyleneterephthalate (PBT) which includes intimately mixing the PET and PBT at a weight ratio of about 10:90-90:10, melting the mixture at 290°-330° C., cooling the mixture to 0°--194° C. by extruding it onto rollers maintained in a cooling bath and orienting the polymer of the resulting continuous shaped object at room temperature to a draw ratio of about 5:1, with subsequent annealing at about 120°-180° C. for about one hour.
机译:一种制备聚对苯二甲酸乙二酯(PET)和聚对苯二甲酸丁二酯(PBT)的均质无定形聚合物共混物的方法,该方法包括以约10:90-90:10的重量比将PET和PBT均匀混合,在290°-330°熔化该混合物C.通过将混合物挤出到保持在冷却浴中的辊上并将混合物在室温下定向到所得连续成型物体的聚合物至约5:1的拉伸比,将混合物冷却至0°-194°C在约120℃-180℃下退火约一小时。