A method of making a niobium activated yttrium tantalate x-ray phosphor using a lithium chloride-lithium sulfate eutectic flux is disclosed. The mole ratio of the flux is 46.5 mole percent lithium chloride to 53.5 mole percent lithium sulfate. Use of this flux improves phosphor brightness by up to 18%, reducing the x-ray dosage to the patient.