PURPOSE:To apply strong and thin ceramic coating having abrasion resistance, corrosion resistance, heat resistance and long life by painting the surface of a metal with a solution consisting of a reaction solution having a specific composition and org. paint and drying the painting layer before baking the same at a relatively low temp. CONSTITUTION:A solution consisting of a sol/gel method reaction solution consisting of metal alkoxide, water and a reaction inhibitor and usual org. paint is applied to a partener material and the painting layer is baked at a relatively low temp. For example, a truck cabin 1 is transported along a hanging rail 5 to stop directly above a painting solution tank 6 and immersed in the painting solution tank 6 and subsequently drawn up to be sent to a drying process to be baked herein at a relatively low temp. At this time, the sol/gel method reaction solution and the org. paint mutually form a solution in the tank 6 and the rapid reaction forming metal oxide due to hydrolysis is appropriately suppressed by the action of the reaction inhibitor and a thin ceramic film is formed.
机译:用途:通过使用由具有特定组成和有机物的反应溶液组成的溶液在金属表面涂漆,以涂覆具有耐磨性,耐腐蚀性,耐热性和长寿命的坚固而薄的陶瓷涂层。在相对较低的温度下烘烤之前,对涂料进行油漆和干燥。组成:一种由溶胶/凝胶法反应溶液组成的溶液,该溶液由金属醇盐,水和一种反应抑制剂以及通常的有机溶剂组成。将油漆施加到伴侣材料上,然后在相对较低的温度下烘烤油漆层。例如,卡车驾驶室1沿着吊轨5被运输以停在涂料溶液罐6的正上方并浸入涂料溶液罐6中,随后被拉起以送至干燥过程以在较低的温度下在此处烘烤。温度这时,溶胶/凝胶法反应液和有机玻璃。涂料在罐6中相互形成溶液,并且通过反应抑制剂的作用适当地抑制了由于水解引起的快速反应形成的金属氧化物,并形成了薄陶瓷膜。

著录项

  • 公开/公告号JPH0389973A

    专利类型

  • 公开/公告日1991-04-15

    原文格式PDF

  • 申请/专利权人 MITSUBISHI MOTORS CORP;

    申请/专利号JP19890224959

  • 发明设计人 HAYAKAWA KAZUTOSHI;

    申请日1989-08-31

  • 分类号B05D7/14;B05D7/24;C23C30/00;

  • 国家 JP

  • 入库时间 2022-08-22 06:01:06

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号